In-phase and Out-of-phase Axial-torsional Fatigue Behavior of Haynes 188 at 760 C

In-phase and Out-of-phase Axial-torsional Fatigue Behavior of Haynes 188 at 760 C
Author :
Publisher :
Total Pages : 26
Release :
ISBN-10 : NASA:31769000601073
ISBN-13 :
Rating : 4/5 (73 Downloads)

Book Synopsis In-phase and Out-of-phase Axial-torsional Fatigue Behavior of Haynes 188 at 760 C by :

Download or read book In-phase and Out-of-phase Axial-torsional Fatigue Behavior of Haynes 188 at 760 C written by and published by . This book was released on 1991 with total page 26 pages. Available in PDF, EPUB and Kindle. Book excerpt:


In-phase and Out-of-phase Axial-torsional Fatigue Behavior of Haynes 188 at 760 C Related Books

In-phase and Out-of-phase Axial-torsional Fatigue Behavior of Haynes 188 at 760 C
Language: en
Pages: 26
In-Phase and Out-of-Phase Axial-Torsional Fatigue Behavior of Haynes 188 Superalloy at 760°C
Language: en
Pages: 18
Authors: PJ. Bonacuse
Categories: Axial-torsional fatigue
Type: BOOK - Published: 1993 - Publisher:

DOWNLOAD EBOOK

Isothermal, in-phase and out-of-phase axial-torsional fatigue experiments have been conducted at 760°C on uniform gage section, thin-walled tubular specimens o
Cyclic Deformation Behavior of Haynes 188 Superalloy Under Axial-Torsional, Thermomechanical Loading
Language: en
Pages: 16
Authors: S. Kalluri
Categories: Axial-torsional
Type: BOOK - Published: 2003 - Publisher:

DOWNLOAD EBOOK

Four types of axial-torsional, thermomechanical fatigue experiments have been performed on Haynes 188 superalloy: mechanically in-phase and thermally in-phase,
NASA Technical Memorandum
Language: en
Pages: 492
Authors:
Categories: Aeronautics
Type: BOOK - Published: 1994 - Publisher:

DOWNLOAD EBOOK

Elevated Temperature Axial and Torsional Fatigue Behavior of Haynes 188
Language: en
Pages: 26
Authors: National Aeronautics and Space Administration (NASA)
Categories:
Type: BOOK - Published: 2018-07-02 - Publisher: Createspace Independent Publishing Platform

DOWNLOAD EBOOK

The results of high-temperature axial and torsional low-cycle fatigue experiments performed on Haynes 188, a wrought cobalt-base superalloy, are reported. Fatig