Cyclic Deformation Behavior of Haynes 188 Superalloy Under Axial-Torsional, Thermomechanical Loading
Author | : S. Kalluri |
Publisher | : |
Total Pages | : 16 |
Release | : 2003 |
ISBN-10 | : OCLC:1251659957 |
ISBN-13 | : |
Rating | : 4/5 (57 Downloads) |
Download or read book Cyclic Deformation Behavior of Haynes 188 Superalloy Under Axial-Torsional, Thermomechanical Loading written by S. Kalluri and published by . This book was released on 2003 with total page 16 pages. Available in PDF, EPUB and Kindle. Book excerpt: Four types of axial-torsional, thermomechanical fatigue experiments have been performed on Haynes 188 superalloy: mechanically in-phase and thermally in-phase, mechanically in-phase and thermally out-of-phase, mechanically out-of-phase and thermally in-phase, and mechanically out-of-phase and thermally out-of-phase. In this study, representative cyclic deformation behavior of the axial-torsional, thermomechanical experiments is presented and compared with isothermal experiments performed at the two temperature extremes (316°C and 760°C) of the thermal cycle. The evolution of cyclic hardening under axial-torsional, thermomechanical conditions is also presented and compared with the corresponding isothermal data.